Name : High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate
Material : Nickel Chromium Iron
Ni (Min) : 50~55%
Density : 8.24 g/cm3
Melting point : 1260-1320°C
Elongation (≥ %) : 25 %
Thermal conductivity : 15.9 W/m·K
Finishing : Bright,Oxided, acid white
Application : Construction, Industry Oil, piping systems
Yield strength : 550MPa
Tensile strength : 910 MPa
Hardness : ≤ 363 HB
Standard : ASTM, ASME
size : 6~200mm
shape : Round, Square, flat
Inconel 718 Alloy
Inconel 718 is a precipitation hardened nickel-based alloy designed to display exceptionally high yield, tensile and creep-rupture properties at temperatures up to 1300°F (704°C). The age-hardening response of Inconel 718 permits annealing and welding without spontaneous hardening during heating and cooling. Nickel Alloy 718 has excellent weldability when compared to the nickel-base super alloys hardened by aluminum and titanium.
Advantages of Inconel 718 Strips
Applications of Inconel 718 Strips
Chemical Properties of Inconel 718
Nickel (plus Cobalt) .......................................................50.00-55.00
Chromium......................................................................17.00-21.00
Iron .....................................................................................Balance
Niobium (plus Tantalum)....................................................4.75-5.50
Molybdenum .....................................................................2.80-3.30
Titanium.............................................................................0.65-1.15
Aluminum ..........................................................................0.20-0.80
Cobalt ...............................................................................1.00 max.
Carbon..............................................................................0.08 max.
Manganese .......................................................................0.35 max.
Silicon ...............................................................................0.35 max.
Phosphorus.....................................................................0.015 max.
Sulfur...............................................................................0.015 max.
Boron ..............................................................................0.006 max.
Copper..............................................................................0.30 max
Density | 8.19g/cm³ | 0.296 lb/in³ |
Melting point | 1260-1336 | 2437°F |
Inconel series
Customize size as below
Shape | Size(mm) |
WIre | 0.5-7.5 |
Rod/Bar | 8.0-200 |
Strip | (0.5-2.5)*(5-180) |
Tube | custom made |
Plate | custom made |
contact us
email:victory@dlx-alloy.com
Oem service:
Welcome customized size
We are experience factory for OEM&ODM service
![]() |
High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate Images |