Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe

  • 1
  • 2
  • 3

Brand Name : Victory

Model Number : Inconel 600

Certification : ISO9001 ROHS

Place of Origin : China

MOQ : 30 Kg

Price : Negotiable

Payment Terms : L/C, T/T, Western Union, MoneyGram

Supply Ability : 300 tons per month

Delivery Time : 20~40 Days

Packaging Details : Inconel 600 rod packed in Spool Carton box, Coil package with polybag,then in woodencase

Name : Excellent corrosion resistant superalloy nickel chrome inconel 600 seamless tube welded pipe

Material : Nickel Chromium Iron

Ni (Min) : 72%

Density : 8.47 g/cm3

Melting point : 1,370-1,425°C

Elongation (≥ %) : 30 %

Thermal conductivity : 15.9 W/m·K

Finishing : Bright,Oxided

Application : Construction, Industry Oil, piping systems

Yield strength : 240 MPa

Tensile strength : 550 MPa

Hardness : ≤ 160 HB

Standard : ASTM, ASME

size : 6~500mm

shape : Round, Square, Seamless, Welded

Contact Now

The performance characteristics of Inconel 600 tube


Excellent corrosion resistance: Inconel 600 has outstanding corrosion resistance, capable of withstanding many corrosive environments, such as the chemical industry, marine environments, and high temperature environments.

High temperature resistance: Inconel 600 tubing can be used for long-term service at temperatures up to 1100°C, making it suitable for high temperature industrial applications.

Good mechanical properties: Inconel 600 tubing has relatively high strength, toughness and fatigue performance, able to withstand high mechanical stresses.

Low thermal expansion coefficient: Inconel 600 has a low thermal expansion coefficient, which is beneficial for maintaining dimensional stability of the tubing under temperature variations.

Excellent oxidation resistance: Inconel 600 tubing can form a dense oxide layer at high temperatures, effectively preventing further oxidation of the inner metal.

The differences between seamless and welded tubing/pipes


Manufacturing process:
Seamless tubes are produced by piercing a solid billet or ingot and then further reducing the diameter and increasing the length.
Welded tubes are formed by bending a flat metal sheet/strip and joining the edges together using a welding process.


Structural integrity:
Seamless tubes have a more uniform and continuous structure without any welded seams.
Welded tubes have a welded joint along the length, which can be a potential weak point.


Surface quality:
Seamless tubes generally have a smoother and more uniform surface finish.
Welded tubes may have some surface irregularities along the weld line.


Strength and toughness:
Seamless tubes typically have higher strength and impact toughness compared to welded tubes.
The weld joint in welded tubes can be a point of weakness.


Cost and availability:
Seamless tubes are generally more expensive to manufacture than welded tubes.
Welded tubes are often more readily available and can be produced in a wider range of sizes and shapes.

Parameter:

Chemical Properties of Inconel 600

C Cr Ni+Co Al Ti Fe Nb+Ta Mn Si P S Cu
≤0.15 14.0~17.0 ≥72 ≤0.35 ≤0.50 6.0~10.0 ≤1.0 ≤1.0 ≤0.5 ≤0.04 ≤0.015 ≤0.5

ITEM θ/℃ TENSIE STRENGTH HBS
σb/MPa σP0.2/MPa δ5/% φ/%
BAR/ROD 20 ≥585 ≥240 ≥30 - 134~217
RING 20 ≥520 ≥205 ≥35 - ≥187
HOT ROLL PLATE 20 ≥550 ≥240 ≥35 ≥40 -
900 ≥95 ≥45 ≥40 ≥50 -
COLD ROLLED SHEET 20 ≥550 ≥240 ≥30 - -
900 ≥90 ≥40 ≥60 - -
COLD ROLLED SHEET 20 ≥550 ≥200 ≥30 - -
STRIP 20 ≥550 ≥240 ≥30 - -
WIRE 20 - HV≤151

Shape
Size(mm)
WIre
0.5-7.5
Rod/Bar
8.0-200
Strip
(0.5-2.5)*(5-180)
Tube
custom made
Plate
custom made

contact us

email:victory@dlx-alloy.com

Oem service:
Welcome customized size
We are experience factory for OEM&ODM service

Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded PipeExcellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded PipeExcellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe


Product Tags:

welded pipe inconel 600 seamless tube

      

Corrosion Resistant Inconel 600 Seamless Tube

      

Superalloy Inconel 600 Seamless Tube

      
China Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe wholesale

Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Changzhou Victory Technology Co., Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)